This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2021, 12, 593–606, doi:10.3762/bjnano.12.49
Figure 1: X-ray diffraction patterns of Pt/C materials.
Figure 2: Micrographs of Pt/C samples of the catalysts G20 (a,b), G25 (c,d), G30 (e,f), G35 (g,h), G40 (I,j),...
Figure 3: Histograms of nanoparticle distribution by the number of intersections with "neighbors" (a–e) and a...
Figure 4: Cyclic voltammograms of Pt/C samples. Sweep rate of 20 mV·s−1, 2nd cycle. Electrolyte used: 0.1 M H...
Figure 5: (a) Linear voltammograms of the ORR. The rotation speed of the disk is 1600 rpm−1, (b) j−1 - ω−0.5 ...
Figure 6: Cyclic voltammograms of (a) G40 and (b) JM40 catalysts measured at a potential sweep rate of 20 mV·s...
Figure 7: Dependence of the ESA of the catalysts on the number of stress test cycles.
Figure 8: Micrographs of Pt/C samples of catalysts G20 (a,b) and JM20 (c,d) after stress test and histograms ...
Figure 9: Histograms of nanoparticle distribution by the number of intersections with "neighbors" for the cat...